The metal/ceramic interface that constitutes an important part of the plasma‐sprayed HA‐coated Ti‐6Al‐4V system may, in fact, represent the “weak link” in the implant design. A post‐plasma‐spray heat treatment to enhance chemical bonding at the metal/ceramic interface and, hence, improve the mechanical properties (interface fracture toughness and tensile coating adhesion strength) of the plasma‐sprayed implant system does show promise. In preliminary heat treatment studies, however, any improvements realized were lost due to the chemical instability of the coating in a moistureladen environment, with a concomitant loss in bonding properties. This deterioration in properties appears to be related to environmentally assisted crack growth as influenced by processing conditions. Still, an ability to improve HA/Ti‐6Al‐4V bonding through enhanced diffusion bonding was demonstrated, warranting further heat treatment studies involving atmosphere control during processing. © 1993 John Wiley & Sons, Inc.

Idioma originalEnglish
Páginas (desde-hasta)191-198
Número de páginas8
PublicaciónJournal of Biomedical Materials Research
Volumen27
N.º2
DOI
EstadoPublished - feb. 1993
Publicado de forma externa

ASJC Scopus Subject Areas

  • Biomaterials
  • Biomedical Engineering

Huella

Profundice en los temas de investigación de 'Post‐plasma‐spraying heat treatment of the HA coating/Ti‐6Al‐4V implant system'. En conjunto forman una huella única.

Citar esto